How many rolls on a pallet of a product?
Usually 20 rolls for Granulated & 23 rolls for smooth.
|
|
How many pallets to a truck load?
If all torch or mop it's 22 pallets to a truck load. If all SA it's 26 pallets to a truck load. If it's a mix of SA & mop or torch it's 23-25 pallets.
|
|
What's the lead time on a specific product?
Please contact Customer Service
|
|
What is a certain product a stock item?
Please contact Customer Service
|
|
What type of adhesive should I be using when installing your modified products?
Polyglass 2000 MB+ SBS Modified Bitumen Mastic-Trowel Grade.
|
|
I have TU Plus installed on my roof, how long can it be left exposed?
Maximum Exposure time is 120 days
|
|
What happens after the allowed exposure time on my Polyglass underlayment?
The use of Polyprotector UDL or Elastobase Poly/Sand properly nailed and another layer of Polystick material properly adhered is recommended.
|
|
Can Polystick TU Plus be used as a metal underlayment?
Yes, POLYGLASS USA accepts the application of TU Plus as a metal underlayment
|
|
Can I torch an APP, or mop an SBS Cap sheet to your Elastoflex SA V Self-Adhered Base Sheet?
Yes, you can torch or mop an approved cap or mid-ply sheet to Elastoflex SA V
|
|
Do I need to prime the drip edge when installing your modified products?
Yes, all metal should be primed using POLYGLASS 100A ASTM D-41 Asphalt Primer
|
|
Is the use of cant strips required by POLYGLASS?
Yes, POLYGLASS requires the use of cant strips at all angle changes, with all POLYGLASS membranes used in low-sloped commercial projects. It is also recommended on residential projects as well.
|
|
With a Polystick TU or TU Plus application, do I need to use modified adhesive during installation?
Yes, all granular to granular, or fabric to fabric laps, must be set in a bed of modified mastic – minimum overlap is 6 inches. Also, all flashing, detail work and tie-ins must be preformed using the POLYGLASS 2000 MB+
|
|
Is there a Warranty on Polystick Products?
Yes, all POLYGLASS Polystick products when properly installed are covered by a 10yr. Limited Roofing Material Warranty.
|
|
Does POLYGLASS have a preferred applicator program?
Yes, POLYGLASS does have a Registered Contractor Program. Please contact the Technical Services Department for additional information.
|
|
I installed Elastoflex SA V Base Sheet as a dry-in. How long can I let it exposed before adhering a cap sheet?
The maximum exposure time is 30 days. Please note: In severe warm weather it is possible that the Polyolefin film with lay lines printed on the top surface may start to yellow and crack due to UV degradation. If this occurs, it is necessary to clean and prime the surface with an A.S.T.M. D-41 Asphalt primer, such as POLYGLASS 100A.
|
|
What is the minimum roof slope required for installation of POLYGLASS products?
A minimum roof slope of ¼': 12 is recommended for POLYGLASS roofing membranes to maximize long-term performance of the roof system and to facilitate adequate removal of water.
|